摘要:
Al-alloy containing Si, Fe, Cu and Mg and at least one kind of Mn and Co in the basic composition range of 8.0≤Si≤30.0 wt. %, 2.0≤Fe≤33.0 wt. %, 0.8≤Cu≤7.5 wt. %, 0.3≤Mg≤3.5 wt. %, 0.5≤Mn≤5.0 wt. % and 0.5≤Co≤3.0 wt. %, are provided in a powder state. A sindered member formed of these Al-alloys has a high strength and reveals excellent heat-resistivity and stress corrosion cracking resistivity. A structural member made of the sintered all-alloy is manufactured through the steps of subjecting a powder press-shaped body formed at a temperature of 350° C. or lower and at a pressure of 1.5.about.5.0 ton/cmto hot extrusion working at a temperature of 300°.about.400° C. to form a raw material for forging, and then forge shaping the raw material at a temperature of 300°.about.495° C.